WIRE FLAME SPRAY torches

GTV COATING TORCHES
FOR THE WIRE FLAME SPRAY PROCESS

5K
Fuel gas:
Acetylene, < 1,4 bar, < 30 l/min
Propane, < 4 bar, < 20 l/min
MAPP, < 4 bar, 20 l/min
Oxygen, < 4 bar, < 100 l/min
Compressed air, < 6 bar, < 0,7 m3/min
Processable spray materials:
Wire / massive wire
Feed rate:
< 1400 g/min (babbitt)  /  < 60 g/min (molybdenum)
Deposition efficiency:
< 90 %

Adhesive wear protection (molybdenum)

 

Sputtering target production

 

Metallization of plastics

 

White metal bearing coatings

7K
Brenngas:
Acetylene, < 1,4 bar, < 30 l/min
Propane, < 4 bar, < 20 l/min
MAPP, < 4 bar, 20 l/min
Oxygen, < 4 bar, < 100 l/min
Compressed air, < 6 bar, < 0,7 m3/min
Processable spray materials:
Wire / massive wire
Feed rate:
< 1400 g/min (babbitt)  /  < 60 g/min (molybdenum)
Deposition efficiency:
< 90 %

Adhesive wear protection (molybdenum)

 

Sputtering target production

 

Metallization of plastics

 

White metal bearing coatings

12E
Brenngas:
Acetylene, < 1,4 bar, < 30 l/min
Propane, < 4 bar, < 20 l/min
MAPP, < 4 bar, 20 l/min
Oxygen, < 4 bar, < 100 l/min
Compressed air, < 6 bar, < 0,7 m3/min
Processable spray materials:
Wire / massive wire
Feed rate:
< 1400 g/min (babbitt)  /  < 60 g/min (molybdenum)
Deposition efficiency:
< 90 %

On-site repair coatings (manual)

15E
Brenngas:
Acetylene, < 1,4 bar, < 30 l/min
Propane, < 4 bar, < 20 l/min
MAPP, < 4 bar, 20 l/min
Oxygen, < 4 bar, < 100 l/min
Compressed air, < 6 bar, < 0,7 m3/min
Processable spray materials:
Wire / massive wire
Feed rate:
< 1400 g/min (babbitt)  /  < 60 g/min (molybdenum)
Deposition efficiency:
< 90 %

On-site repair coatings (manual)

 

Adhesive wear protection (molybdenum)

 

Metallization of plastics

 

White metal bearing coatings